From a thin film to an insulating char: the chemistry and physics of intumescent coatings in a fire, and why expansion and performance are specific to each product.

World Steel 工程团队 · 更新于 2026-10-16 · 阅读约 2 分钟

Intumescent coating expanding into char (illustration)

Three ingredients working together

A typical intumescent formulation contains an acid source (often a phosphate), a carbon source (a polyol) and a blowing agent (for example a melamine compound), held in a binder that softens when heated.

  1. The binder softens and the acid source decomposes.
  2. The acid reacts with the carbon source to form a carbon-rich char.
  3. The blowing agent releases gases that foam the softened mass.
  4. The result is a thick, porous char with low thermal conductivity.

The degree of expansion, the char strength and the insulation are specific to each product and are only known from its fire tests.

What the char does

The char is an insulating blanket between the fire and the steel. Heat still passes through, but much more slowly, so the steel temperature rises gradually. The coating is designed so that the steel stays below its critical temperature for the rated time.

Cellulosic and hydrocarbon fires

Building fires follow the standard (cellulosic) fire curve – ISO 834, ASTM E119, AS 1530.4. Hydrocarbon pool fires heat up much faster and hotter (UL 1709, EN 1363-2), and jet fires add erosion. Thin-film building intumescents are not designed for these conditions – epoxy systems tested for hydrocarbon and jet fires are.

What decides performance

  • Dry film thickness – more coating, more char.
  • Section factor – how fast the member heats up.
  • Critical steel temperature – the target the steel must stay below.
  • Section shape – open sections and hollow sections are tested separately.

FAQ

At what temperature does intumescent coating start to expand?

Typically from around 200–250 °C, but the exact activation temperature depends on the product.

Does the char fall off?

A correctly applied and certified system keeps a stable char for the tested duration; char stickability is part of the fire test.

需要您项目的涂层厚度和成本?发送构件清单和耐火等级 – 我们的工程师将编制防火保护方案。
索取方案

Preliminary calculations are provided for estimation purposes only. Final coating thickness and fire protection system selection must be verified against the approved product documentation, applicable project requirements and relevant engineering assessments.

下一个项目

计划在海外建造钢结构?

请发送您的图纸或 IFC 模型——我们的报价团队将回复加工范围、工期及到岸价格。