- SUS304 (1.4301) and SUS316 (1.4401) grades
- No coating to chip, flake or contaminate
- Pickled and passivated after welding
- Same WS sizes, meshes and codes
Why stainless
Stainless steel grating needs no coating, cleans easily and resists corrosion where galvanised steel would be attacked – food and beverage, dairy, pharmaceutical, chemical plants, water and wastewater treatment, coastal and marine structures. SUS304 suits most hygienic and indoor uses; SUS316, with molybdenum, is chosen for chlorides, sea water and aggressive chemicals.
Fabrication
- Separate tools and storage from carbon steel to prevent iron contamination.
- Welded with matching stainless filler; heat tint removed by pickling.
- Passivated and rinsed; surface finish agreed for hygienic areas.
- Fasteners and clips in stainless steel of the same or better grade.
Load capacity is similar to carbon steel grating of the same size for selection purposes; final design uses the stainless steel properties of the project code (for example AISC Design Guide 27, AS/NZS 4673 or EN 1993-1-4).
各市场标准与要求
World Steel 设计、加工本产品及编制文件所依据的规范——以及各市场的主要几何与荷载要求。
美国
- ASTM A240 / A276Stainless plate, strip and bars
- ASTM A380 / A967Cleaning, descaling and passivation
- AISC Design Guide 27Structural stainless steel
澳大利亚 / 新西兰
- AS/NZS 4673Cold-formed stainless steel structures
- AS 1657Platforms and walkways
欧洲
- EN 10088Stainless steels
- EN 1993-1-4Stainless steel design
- EN ISO 14122-2Working platforms and walkways
摘要仅供参考——以项目技术规格书、所采用的规范版本及主管机构要求为准。
表面处理
| 表面处理 | 标准 / 备注 |
|---|---|
| Pickled & passivated | ASTM A380 / A967 or equivalent |
| Electropolished | On request for hygienic areas |
常见问题
SUS304 or SUS316?
SUS304 for general hygienic and indoor use; SUS316 where chlorides, sea water or aggressive chemicals are present.
Can stainless grating be mixed with galvanised frames?
Yes, with isolating washers or sleeves where needed to avoid galvanic corrosion in wet conditions.